Chemical Composition | |||||||||
Alloy series | Si | Fe | Cu | Mn | Mg | Cr | Zn | Ti | |
5083T | Min. | - | - | - | 0.40 | 4.0 | 0.05 | - | - |
Max. | 0.40 | 0.40 | 0.10 | 1.0 | 4.90 | 0.25 | 0.25 | 0.15 | |
5182T | Min. | - | - | - | 0.20 | 4.0 | - | - | - |
Max. | 0.20 | 0.35 | 0.15 | 0.50 | 5.0 | 0.1 | 0.25 | 0.1 | |
5454T | Min. | - | - | - | 0.5 | 2.4 | 0.05 | - | - |
Max. | 0.25 | 0.40 | 0.10 | 1.0 | 3.0 | 0.20 | 0.25 | 0.20 |
Alloy Series | Thickness(mm) | Width(mm) | Length(mm) | |
5083T | Min. | 4 | 1000 | 2000 |
Max. | 8 | 2400 | 12600 | |
5182T | Min. | 4 | 1000 | 2000 |
Max. | 8 | 2400 | 12600 | |
5454T | Min. | 4 | 1000 | 2000 |
Max. | 8 | 2400 | 12600 |
Alloy Series | Temper | Yield Strength Rp(Mpa) |
Tensile Strength Rm(Mpa) | Elongation A(%) |
5083T | O, H111, H112 |
≥125 ≥125 |
270-350 ≥275 |
≥15 ≥12 |
5182T | O, H111 | ≥110 | 255-315 | ≥16 |
5454T | O, H111, H112, H32 |
≥85 ≥125 ≥180 |
215-275 ≥220 250-305 |
≥17 ≥8 ≥8 |